UPR Unsaturated Polyester Resin Hand Lay - Up For Fiber - Reinforced Plastic FRP
Product Details:
Place of Origin: | China |
Brand Name: | B&W |
Certification: | ISO 9001, ISO 14001 |
Model Number: | Hand Lay-up and others |
Payment & Shipping Terms:
Minimum Order Quantity: | As need |
---|---|
Price: | Negotiable |
Packaging Details: | In 220kg drums |
Delivery Time: | 2 weeks |
Payment Terms: | T/T, L/C |
Supply Ability: | As need |
Detail Information |
|||
Appearance: | Viscous Liquid | Type: | General Level |
---|---|---|---|
Excuting Standard: | GB/T 7193.1-2008 | Hazard Class: | None |
Package: | 220KG Drum | Shelf Life: | 3 Months Below 25°C |
High Light: | upr unsaturated polyester resin,liquid polyester resin |
Product Description
UPR Unsaturated Polyester Resin Hand Lay - Up For Fiber - Reinforced Plastic FRP
Hand Lay - Up Resins Unsaturated Polyester Resin For Fiber - Reinforced Plastic FRP
Product Name | Type | TypeViscosity(25℃,cps) | Gel time(℃) | Characteristics and Applications |
HS-1101S | PTA | 90-120 | - | Pre-accelerated, thixotropic, well-spliced with acrylic. Suitable for hand lay-up and spray-up of FRP reinforcement parts for acrylic sanitary wares. |
HS-1101PT Series | PTA | 70-100 | - | Pre-accelerated, thixotropic, well-spliced with acrylic. Suitable for hand lay-up and spray-up of FRP reinforcement parts for acrylic sanitary wares. |
HS-1071 | Ortho | 250-600 | 10.0-55.0 | Thixotropic, pre-accelerated, excellent workability. Quickly curing properties, quick de-moulding. Suitable for general purpose. |
HS-1102 |
Ortho | 200-500 | 10.0-50.0 | Approved by Lloyds’ Register and CCS for boat building, thixotropic, pre-accelerated,excellent water resistance ,low exotherm, excellent workability. Suitable for applications of FRP boats and other thick or large dimensional FRP products. |
HS-1102AB/AC/AD |
Ortho | - | - | Designed particularly for different bathtubs of bonding layer. (ABS/acrylic panel/acrylic or ABS compound panel) |
HS-1102TC Series |
Ortho | 160-250 | 45.0-55.0 | Medium reactivity, thixotropic, pre-accelerated, containing wax and curing indicator, with long gel time and low exotherm. Excellent water resistance and mechanical strength. Suitable for hand lay-up or spray-up application of products with large dimensions, such as FRP cabin cover, boat building, cooling towers etc. |
HS-1102PT |
Ortho | 70-100 | - | Pre-accelerated, thixotropic, well-spliced with acrylic. Suitable for hand lay-up and spray-up of FRP reinforcement parts for acrylic sanitary wares. |
HS-1105 Series | Ortho | 400-650 | 15.0-55.0 | Medium reactivity, thixotropic, pre-accelerated, containing wax and curing indicator, with long gel time and low exotherm. Excellent water resistance and mechanical strength. Suitable for hand lay-up or spray-up application of products with large dimensions, such as FRP cabin cover, boat building, cooling towers etc. |
HS-189 |
Ortho | 330-480 | 20.0-35.0 | Approved by CCS for boat building, with excellent water resistance, excellent toughness. Suitable for boat building, cooling towers. |
HS-196 |
Ortho | 700-1100 | 25.0-35.0 | Approved by CCS for boat building, excellent toughness and mechanical properties. Suitable for transportation applications. |
HS-197 | BPA/UPR | 400-600 | 10.0-30.0 | It has a excellent chemical resistance, and a significant alkali resistance compared to other unsaturated polyester resin. It has a higher heat distortion temperature, suitable for hand lay-up FRP pipes, containers, storage tanks and other equipments. |
HS-199 | ISO | 650-850 | 15.0-25.0 | excellent heat,acid resistance and electric properties. Suitable for chemical equipments and other FRP products which high heat resistance required. |
HS-2103 | Ortho | 300-500 | 80.0-110.0 | Thixotropic, pre-accelerated, LSE resin with long gel time and low exothermic temperature allowing for application of thick laminates wet-on-wet. excellent heat resistance and mechanical properties. Suitable for hand layup or spray-up application of products requiring high strength with large dimensions, such as wind mill blades. |
HS-2138HL | ISO | 400-550 | 10.0-24.0 | Medium reactivity, has excellent comprehensive mechanical properties, dimension stability is excellent, suitable for hand layup process production boats, auto parts, cooling towers and other FRP products. |
HS-2239 | PTA | 400-600 | 10.0-20.0 | Low viscosity, excellent wet-out characteristics, low volatilization of styrene. excellent heat resistance and electrical properties, high mechanical strength, suitable for producing medium and small vehicles, yachts, and GRP/FRP products. |
HS-4430 |
VE | 400-500 | 10.0-30.0 | High mechanical strength and toughness, the composite product made of it shows excellent long-term heat- resistance and because of smAll sensitivity to stress, it exhibits higher dynamic load bearing capacity. It has significant resistance to chemical corrosion(inorganic acid, alkali, salt), suitable for hand lay-up/winding/ pultrusion process to manufacture FRP pipelines, containers, storage tanks, chemical equipments and the FRP moulds. |
HS-4431 | VE | 300-500 | 7.0-27.0 | Intended for high strength, high toughness and corrosion resistance FRP products as well as paints and adhesives used for anti-corrosion engineering, especiAlly suitable for hand lay-up, winding, pultrusion process. Glass flake coating cement, winding chemical pipelines, corrosion-resistant floors and winding tank corrosion and so on. |
HS-4432 | VE | 400-600 | 10.0-20.0 | Has excellent acid, alkali, water, and organic solvent resistance, applied for FRP tanks, containers, pipes, corrosion-resistant flooring and chemical devices that need to be protected, such as pulp mill equipment. Appropriate process for this resin: hand lay-up , FRP lining, flake lining, compression molding, gas bag molding, pultrusion filament winding process and so on. |
HS-4433 |
VE | 300-500 | 8.0-18.0 | Optimized heat generation rate of curing and exothermic peak temperature. It is the standard grade of Huake vinyl ester resin. It has high mechanical strength and excellent toughness, the composite product made of it shows excellent long-term heat resistance, smAll sensitivities to stress, so it exhibit higher dynamic load bearing capacity, and has a better resistance to a wide range of acid, alkali, salts, organic solvents. Suitable for hand lay-up, winding and pultrusion, casting, RTM and many other FRP process to manufacture anti-corrosive FRP lining, overAll FRP tanks, pipes, towers, tanks, grating, chemical equipments and products, electrical insulation materials, glass molds. |
HS-4439 | VE | 300-500 | 10.0-30.0 | Has excellent flexibility, high elongation properties, also has excellent fatigue resistance, impact resistance and crack resistance. Suitable for making kinds of sporting equipments, safety helmet and other equipments which need shock resistance, fatigue resistance, especiAlly suitable for hand lay-up, winding, pultrusion process. |
HS-4457 |
VE | 250-450 | 10.0-30.0 | Compared to HS-4451 resin, HS-4457 is more suitable for manufacturing FRP products, and widely used for acids, alkalis, salts, organic solvents and other chemicals in chemical engineering and industries. It is an ideal anti-corrosive FRP resin. |
HS-2005 | AA | 500-700 | 8.0-18.0 | Excellent flexibility with high elongation. Suitable for blending. |
HS-2006 | AA | 500-700 | 12.0-22.0 | Excellent flexibility with high elongation. Suitable for blending in decorative bar of furniture and SMC/BMC formulations. |
HS-2007 | Ortho | 500-700 | 10.0-20.0 | excellent flexibility with high elongation. Suitable for blending. |
HS-2010 | ISO | 900-1100 | 15.0-25.0 | Excellent flexibility with high elongation,readily thickened with magnesium oxide. Suitable for blending in SMC/BMC formulations. |
Want to Know more details about this product